Please use this identifier to cite or link to this item:
https://scholarhub.balamand.edu.lb/handle/uob/2104
Title: | The impact of surface roughness and PTFE/TiF3/FeF3 additives in plain ZDDP oil on the friction and wear behavior using thermal and tribological analysis under extreme pressure condition | Authors: | Nehme, Gabi Ghalambor, Saeed |
Affiliations: | Department of Mechanical Engineering | Keywords: | Scanning Electron Microscopy (SEM) ZDDP PTFE Friction Wear |
Subjects: | Catalysts | Issue Date: | 2014 | Part of: | International journal of materials and metallurgical engineering | Volume: | 8 | Issue: | 7 | Start page: | 739 | End page: | 746 | Abstract: | The use of titanium fluoride and iron fluoride (TiF3/FeF3) catalysts in combination with polutetrafluoroethylene (PTFE) in plain zinc- dialkyldithiophosphate (ZDDP) oil is important for the study of engine tribocomponents and is increasingly a strategy to improve the formation of tribofilm and provide low friction and excellent wear protection in reduced phosphorus plain ZDDP oil. The influence of surface roughness and the concentration of TiF3/FeF3/PTFE were investigated using bearing steel samples dipped in lubricant solution at 100°C for two different heating time durations. This paper addresses the effects of water drop contact angle using different surface; finishes after treating them with different lubricant combination. The calculated water drop contact angles were analyzed using Design of Experiment software (DOE) and it was determined that a 0.05 μm Ra surface roughness would provide an excellent TiF3/FeF3/PTFE coating for antiwear resistance as reflected in the Scanning electron microscopy (SEM) images and the tribological testing under extreme pressure conditions. Both friction and wear performance depend greatly on the PTFE/and catalysts in plain ZDDP oil with 0.05 % phosphorous and on the surface finish of bearing steel. The friction and wear reducing effects, which was observed in the tribological tests, indicated a better micro lubrication effect of the 0.05 μm Ra surface roughness treated at 100°C for 24 hours when compared to the 0.1 μm Ra surface roughness with the same treatment. |
URI: | https://scholarhub.balamand.edu.lb/handle/uob/2104 | Open URL: | Link to full text | Type: | Journal Article |
Appears in Collections: | Department of Mechanical Engineering |